Laser Cladding of Shafts

Common damages of shafts

  • Worn out bearing seat
  • Damaged conical seats
  • Damaged sealing seats
  • Worn out grooves, e.g. feather key

Advantages

  • High accuracy
  • No distortion of shaft
  • Manufacturing to original size
  • Locally improved properties due to individual cladding with optimal alloys, e.g. hard phasing alloys, Ni and Co-based alloys

 

For your information: Flyer Laser-Powder-Cladding of Shafts